Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME requirement for 100% RT for stainless steel plates above 38mm

Status
Not open for further replies.

jbesson

Petroleum
Feb 13, 2008
25
Hi dears Specialists

I have in mind a requirement from ASME VIII div 1 about 100% RT for stainless steel plates above 38mm.
I have been able to found the UCS-57 § for CS and the limit of 32mm but impossible to find the § dealing with the limit for stainless steel in the UHA...

Do I start to loose my mind ?

Thanks in advance !
 
Replies continue below

Recommended for you

jbesson, see UW-11, UW-33 Sorry, UHA-33 [headsmack]

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
You were thinking of using E = 0.7 or 0,85 for SS plates above 38 mm ?

Regards
 