Hi,
I have to select an anticorrosion coating for the bends of a 16" offshore pipeline with a design temperature of 35°C. Ambient temperature is 15°C. Design life 50 years.

Designer propose a polyurethane coating system (airlees spray applied) with 5 mm of thickness.
Wath is the best choice between polyurethane coating and epoxy coating?

Is this thickness acceptable?

Thx
 
With epoxy, especially offshore, you might want a poly coating on top for mechanical strength anyway.

**********************
"Pumping accounts for 20% of the world’s energy used by electric motors and 25-50% of the total electrical energy usage in certain industrial facilities."-DOE statistic (Note: Make that 99% for pipeline companies)
 
OK BigInch.

But I have some doubt about the thickness of coating (5 mm).
Data sheet of materials that I encountered in the past gave a maximum thk of 3 mm.

Thx for support!
 
5 mm is not a problem. Perhaps the 3 mm was just a thickness to be applied, not a maximum.

**********************
"Pumping accounts for 20% of the world’s energy used by electric motors and 25-50% of the total electrical energy usage in certain industrial facilities."-DOE statistic (Note: Make that 99% for pipeline companies)
 
Actually 5 mm sounds very thin.

**********************
"Pumping accounts for 20% of the world’s energy used by electric motors and 25-50% of the total electrical energy usage in certain industrial facilities."-DOE statistic (Note: Make that 99% for pipeline companies)
 
The best choice is the one that passes all of the qualification testing that you will, of course, have defined. Thicker does not mean better.

Steve Jones
Materials & Corrosion Engineer
 
Yes, even not having experience with that product, I would tend agree with that, especially noting where he says the thickness of the abrasion resistant FBE (no additional mechanical protection coating) is 150 mm.
5 mm no.

**********************
"Pumping accounts for 20% of the world’s energy used by electric motors and 25-50% of the total electrical energy usage in certain industrial facilities."-DOE statistic (Note: Make that 99% for pipeline companies)
 