Hello,
I am a young mechanical at a aluminum fab shop. We weld most of our connections and I have been having a serious problem with weld contamination from of punch fliud. I realize the importance of cleanliness for aluminum welding but it is essential that I use some type of cutting fluid mixture for our turret punch. Currently we use a mixture of cutting fluid, transmission fluid and water on our punch and then attempt to wipe them down before welding. Needless to say the surface remains somewhat oily. I am looking for suggestions on a different fluid that will not effect the welds or any quick technique we could use to clean the weld areas. Thank you in advance for your time.

DiBlazing
 
For your situation, I would probably purchase a cleaning solvent like that used for nondestructive testing (NDT). We purchase Liquid Penetrant cleaner from the following web site - there are other web sites to purchase Liquid Penetrant cleaner, as well. The cleaner is sprayed on the surface and easily wiped off with a rag, in preparation for Liquid penetrant inspection, but it could also be used for other applications. Removes most surface residue - great for preparing surfaces for inspection and pre-weld cleaning, and is safe to use as well.

 
metengr,
Thank you very much for your time. I do perform destructive testing here, however I do not do any nondestructive testing and was not familiar with the NDT solvents. I looked up that website and it turns out that Magna Corp. is right in my backyard. They are going to send me a sample to give it a try. I truley appreciate it.

Best Regards,
DiBlazing
 
Clean with alcohol and clean rags. The wire brush with stainless steel wire brush.
 