Hi all,
I am designing a pressure piping system where the pipe material is SS to ASTM A 240, TP 904L (UNS N08904). I was trying to decide the corresponding pipe spec and the allowable stresses as per B 31.1 - but am completely confused without any joy.
I noticed ASTM A 312 standard covers pipes to material TPXM-15/ UNS N08904. However B31.1 does not list that type under spec A 312 nor does AutoPipe in its library. From some lirterature on net it appears ASTM B673 & B674 could be appropriate pipe standards for 904L material. Again, B 31.1 doea not list the grade under B673 - and Autopipe does not have any pipe spec for "B" series.
Expecting some of you might have used this piping material in past and will be able to throw some light.
regards,
I am designing a pressure piping system where the pipe material is SS to ASTM A 240, TP 904L (UNS N08904). I was trying to decide the corresponding pipe spec and the allowable stresses as per B 31.1 - but am completely confused without any joy.
I noticed ASTM A 312 standard covers pipes to material TPXM-15/ UNS N08904. However B31.1 does not list that type under spec A 312 nor does AutoPipe in its library. From some lirterature on net it appears ASTM B673 & B674 could be appropriate pipe standards for 904L material. Again, B 31.1 doea not list the grade under B673 - and Autopipe does not have any pipe spec for "B" series.
Expecting some of you might have used this piping material in past and will be able to throw some light.
regards,