What is the general or most common type of 17-4 used in the oil and gas industry, mainly in valve design? 17-4PH or another type.
 
Replies continue below

Recommended for you

It is the PH alloy, either 17-4 or in heavy sections where toughness needed 15-5PH.
Often aged to H1100 or H1150 for better cracking resistance. If you can live with less strength then H1150M overaged is even tougher.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
if Nace requirement is applicable, double aging shall be carried out, which means that the condition H1150DBL or H1150M shall be the one applicable