1000 hr salt spray coating 1

Status
Not open for further replies.

Bob_3

Mechanical
Joined
Feb 20, 2019
Messages
25
Location
US
We have some components that need to meet a 1000 hr salt spray test. Anything thicker than a G90 hot-dipped zinc will make the part not function in use. Other than redesigning the part to accommodate a thick coating, is there any alternative to hdg for a low cost thin coating that will pass the salt spray?

Any info is appreciated...
 
Zinc-aluminum flake coatings such as Dacromet can significantly outperform galvanizing in salt spray. They are thin enough to be applied to nuts and bolts without interfering with threading.

Electroless nickel is supposed to be the best thin coating for corrosion protection but in my experience it works or it fails absolutely. There is never an in-between.
 