INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Hardness Values Reference for Material 1.6368 (15NiCuMoNb5-6-4)

Hardness Values Reference for Material 1.6368 (15NiCuMoNb5-6-4)

Hardness Values Reference for Material 1.6368 (15NiCuMoNb5-6-4)

(OP)
Dear Gents,
Hope you are all well!

I need help finding a reference for the hardness values of Material 1.6368 (15NiCuMoNb5-6-4).


Appreciating your help
Thanks and Regards.
M Elsayed

RE: Hardness Values Reference for Material 1.6368 (15NiCuMoNb5-6-4)

Could you quote a US equivalent?

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."

RE: Hardness Values Reference for Material 1.6368 (15NiCuMoNb5-6-4)

200 to 210 Brinell.ASTM-A182-Grade-F36 is the similar alloy


luis

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login



News


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close