I am planning to install a productionline to "paint" glass bottle to simulate etching glass, I heart that one of the method is powder coating, could somebody help me to identify the equipment we need and the caracteristic of them, i.e, need preheater station? what is the ideal temperature? wich king of guns we must use? what kind of cure procees you recomend (Oven, UV or IR)
Thanks in advance.
rbisca
 
Powder coating is an electro static process. I don't believe the bottles will hold an electro static charge.
 