Dear all experts,

I am trying to simulate the welding process of SA 387 GR Cl 2 material using FEA.

But I need the Yield Stress of SA 387 varied with temperature also I should use yield strength as dependent on time.

Where Can I find out these material Properties?

Best regards...

 
Thank you for your advise Luis.
 
Not sure about time-dependent properties but Table Y-1 in ASME Section II Part D lists the yield strength values of SA-387 Gr11 Cl2 plate from 100°F to 1,000°F.


-Christine
 
Thank you for your advise Chrisine...
 
Dear Experts Yes I have found Yield stresses value dependent on temperature Asme Section II Part D table Y-1 but Could I find tangent modulus?
 