Hello:

I would greatly appreciate if someone can tell me the
yield stress (Fy) and ultimate stress (Fu) values of a steel ASTM A668 grad M.

Thank you and best regards.
 
It varies by thickness. What size forgings are you looking at?

Tim
 
Hello Constructioneer:

Thank you for your responding. The diameter is 6.5 in.

Regards.
 