Apr 9, 2008 #1 camarade Mechanical Joined Sep 14, 2007 Messages 3 Location US Hello: I would greatly appreciate if someone can tell me the yield stress (Fy) and ultimate stress (Fu) values of a steel ASTM A668 grad M. Thank you and best regards.
Hello: I would greatly appreciate if someone can tell me the yield stress (Fy) and ultimate stress (Fu) values of a steel ASTM A668 grad M. Thank you and best regards.
Apr 9, 2008 #2 Constructioneer Structural Joined Mar 29, 2008 Messages 11 Location US It varies by thickness. What size forgings are you looking at? Tim Upvote 0 Downvote
Apr 9, 2008 Thread starter #3 camarade Mechanical Joined Sep 14, 2007 Messages 3 Location US Hello Constructioneer: Thank you for your responding. The diameter is 6.5 in. Regards. Upvote 0 Downvote
Apr 9, 2008 #4 Constructioneer Structural Joined Mar 29, 2008 Messages 11 Location US Yield Point: 115 ksi Min. Tensile: 140 ksi Tim Upvote 0 Downvote