Will I be able to distinguish which identical geometry parts are made of 403F 430F and which are 430FR.
Situation: I had two groups of samples annealed. Unfortunately there appears to have been parts mixed as my two bags of samples no longer contain the same number they went out of with.
My understanding is that these devices are pretty good with Silicon, that being the biggest difference in material composition between these two alloys
david
Situation: I had two groups of samples annealed. Unfortunately there appears to have been parts mixed as my two bags of samples no longer contain the same number they went out of with.
My understanding is that these devices are pretty good with Silicon, that being the biggest difference in material composition between these two alloys
david