robgreg1978
Petroleum
I am fairly new to the qc world although I have been welding for the last 17 years. The paper work sometimes gets to me.
My question is I have a welder that is qualified on 2" xs GTAW all the way out. He also is qualified on 2" xs SMAW 6010 root/ 7018 fill and cap. Does this qualify him to weld a joint that calls for GTAW root/ 7018 fill and cap?