Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Withdrawal Resistance of Lag Screws in Wood

Status
Not open for further replies.

Grunchy

Industrial
Feb 25, 1999
28
Hello,
What effect does "edge distance" have on lag screw withdrawal resistance in wood? I need a source as well, just let me know your source and I'll look it up!

I found in "Standard Handbook of Fastening and Joining" a chart that was reproduced from AF&PA source, wherein a withdrawal strength was related to lag screw diameter and wood specific gravity. Well I know that it also depends on the thread penetration, but I wonder if it matters what the "edge distance" is.

Or maybe it is enough if I specify a minimum "edge distance", such as 4 diameters or 1.5 diameters. For instance, in the same book under lateral loading, if the direction of loading is parallel to the grain the min. edge distance is 1.5 diameters, if the loading is perpendicular to the grain the min. edge distance is 4 diameters.

-= Any Help Is Appreciated =-

Thank you,
"Grunchy" P.E.
 
Replies continue below

Recommended for you

See also ANSI/AF&PA NDS Section 9.4.

For lag screws in withdrawal (no lateral load):
Min. edge dist. = 1.5D
Min. end dist. = 4D
Min. spacing = 4D
 
Much obliged, "boo1" and "Taro"!
The linked resources are indispensible, thank you kindly!
 