Hi
Designing a 25% Commonwealth CA-1 Wirraway flying scale replica.
Need some assistance calculating beam strength of 6061-T6 Aluminium tube which will be used as wing joiners for outer panels to centre section.(The outer panels have to be removable for transport)
Each side (wing panel) will use two poles in parallel, one 1.25” dia located at thickest part of wing section, another of .75” dia just in front of the rear spar.
Both tubes will be 6061 - T6 with .035” wall.
Given the model will weigh approx. 60lbs, will the T6061 tube be up to the task ? and what length of pole would be required to tolerate flying (and landing) stresses.
Other data
Centre Section Wing:-
Span 30.75”
Cord 25.25”
Area (Less Fus)=454 ins2
Outer Wing Panels:-
Span (Less Tips)=48”
Cord at wing joint=25.25”
Cord at tip =12.5”
Area (each)=906 Ins2
Projected weight of model 50 – 55lbs
Thanks and regards
Chris
Designing a 25% Commonwealth CA-1 Wirraway flying scale replica.
Need some assistance calculating beam strength of 6061-T6 Aluminium tube which will be used as wing joiners for outer panels to centre section.(The outer panels have to be removable for transport)
Each side (wing panel) will use two poles in parallel, one 1.25” dia located at thickest part of wing section, another of .75” dia just in front of the rear spar.
Both tubes will be 6061 - T6 with .035” wall.
Given the model will weigh approx. 60lbs, will the T6061 tube be up to the task ? and what length of pole would be required to tolerate flying (and landing) stresses.
Other data
Centre Section Wing:-
Span 30.75”
Cord 25.25”
Area (Less Fus)=454 ins2
Outer Wing Panels:-
Span (Less Tips)=48”
Cord at wing joint=25.25”
Cord at tip =12.5”
Area (each)=906 Ins2
Projected weight of model 50 – 55lbs
Thanks and regards