Will straightening cast steel cause internal stress?
Our supplier is proposing the following process.
Cast steel part, heat treat to hardness spec, and then straighten the part in a form.
Is this going to introduce internal stress that will relax over time?
Is this a standard process for cast parts?
Our supplier is proposing the following process.
Cast steel part, heat treat to hardness spec, and then straighten the part in a form.
Is this going to introduce internal stress that will relax over time?
Is this a standard process for cast parts?