EssieAutomation
Mechanical
I have a titanium weldment (3 pieces, 6Al-4V)which is being used in an ice climbing product. After welding, I am having it sandblasted to give it a nice finish and wish to leave it in this form. In the past, I did not sandblast the weldment, instead I anodized it. My customer now has a concern for corrosion on this weldment - their reason being that since the sandblasting has opened up the pores in the metal, it will in fact rust (is that true?). I personally own titanium products of the same material and finish and have had no ill effects over several years. Should I have this weldment plated or anodized in some way, or are these concerns actually not concerns at all?
Thank you for any help,
Steve
Thank you for any help,
Steve