Hi,

I have two anti-rust products.
This (G-15 Soft film rust Inhibitor oil) is what we currently use but due to shortage we need to find alternative. This (CRC Soft seal heavy film) was only available.

I would like to what I should compare to see the alternative is okay for use.

 
 https://files.engineering.com/getfile.aspx?folder=39e3a8fa-4fab-45a9-b27a-ea871762889e&file=CRC.pdf
Is this just to protect parts sitting on the shelf or will they see worse conditions?
You can't cover or enclose them?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 