Jan 24, 2008 #1 koplan Mechanical Joined Jan 24, 2008 Messages 17 Location KR Field hydrotest is done in new condition. But almost and usually, it's needed to ensure the safety for corroded condition not new in field.
Field hydrotest is done in new condition. But almost and usually, it's needed to ensure the safety for corroded condition not new in field.
Jan 25, 2008 #2 doct9960 Mechanical Joined Aug 15, 2006 Messages 618 Location CA http://www.codeware.com/support/faq/1209.html Upvote 0 Downvote