Dears

My Company wants to take PQR with Material SA-516 according to ASME Sec. IX. for qualification of Gr. No. 1 and 2, I have plan to take PQR with SA-516 Gr. 60 (Gr. No. 1) to SA-516 Gr. 70 (Gr. No. 2) for this purpose.
I found a Triple Grade SA-516 Gr. 60/65/70 in a warehouse with proper thickness, I want to know that which Gr. No. shall be selected and recorded in Qualification record for mentioned material.
If I use this material for both side of PQR, Can I consider this PQR for qualification P no. 1 Gr. No 1 to 2?


 
Yes. See below interpretation. Only one side needs to be impact tested.


Interpretation: IX-92-70R
Subject: QW-403.5, Base Metals
Date Issued: June 4, 2001
File No: 00-470
Question (1): When a procedure qualification with supplemental notch toughness requirement is conducted with one P-Number material having multiple certifications in different Group Numbers, are WPSs qualified for all combinations of the Group Numbers?
Reply (1): Yes.
Question (2): In the above question, does one set of HAZ impact specimens, when required, satisfy the requirements of Section IX?
Reply (2): Yes.
Question (3): When a procedure qualification with supplemental notch toughness requirement is conducted with two materials of different P-Number each having multiple certifications in different Group Numbers, are WPSs qualified for all combinations of the multiple certified Group Number of the first P-Number material to the multiple certified Group Number of the second P-Number material?
Reply (3): Yes.
Question (4): In the above question, does one set of HAZ impact specimens from each P-Number material, when required, satisfy the requirement of Section IX?

Question (5): In Question (3), are materials from the multiple certified Group Numbers qualified for welding a P-Number material to itself?
Reply (5): No.
Note: The term “multiple certifications” as used means any material for which a material test report indicates that the material meets all the requirements of two or more specifications, grades, types, or classes.
 