my company had a training on vessels under cyclic service.
it's advised to consider the following factors in case of fatigue analysis to increase fatigue life:
  1. Vessels to be PWHT(For CS)
  2. All welds be full penetration
  3. Integral construction
  4. Avoid slip on flanges
  5. Avoid leg support
  6. Avoid peaking at Category A joints
i wonder if they are mandatory per ASME VIII-2? i look through the rules in Code, and can't find any basis.
what do you think of these factors?