hi, all,
my company had a training on vessels under cyclic service.
it's advised to consider the following factors in case of fatigue analysis to increase fatigue life:
what do you think of these factors?
Thanks in advance
my company had a training on vessels under cyclic service.
it's advised to consider the following factors in case of fatigue analysis to increase fatigue life:
- Vessels to be PWHT(For CS)
- All welds be full penetration
- Integral construction
- Avoid slip on flanges
- Avoid leg support
- Avoid peaking at Category A joints
what do you think of these factors?