Good Day Everyone,

If this question has already been answered then please direct me to the appropriate thread.

I have recently been tasked with reviewing the material grades currently used for our product designs to make sure they have the needed mechanical properties. To accomplish this I have been cross referencing the mechanical properties in the appropriate ASTM Standards to our design calculations.

I am down to my last two groups of materials and I am having trouble locating what ASTM standards cover the mechanical properties of:

1) 1018 / 1020

2) 4130 / 4140

in both flat and round bars.

If ASTM standards do not clearly cover these materials what SAE standards do.

Thank you in advance for all your help.

 
They are SAE/AISI standard material grades. 4130/4140 are heat treatable grades that can meet a multitude of strength requirements.
Strength of 1018/1020 varies with hot rolled, cold finished or cold drawn/rolled condition.
 
SAE J403 covers chemical composition for 1018/1020. SAE J404 covers chemical composition for 4130/4140. ASTM A29 covers the chemical composition for both. If you want mechanical properties, try one of these:

Hot-Rolled Carbon Steel Bars:
Steel Bars, Carbon, Quenched and Tempered A321
Steel Bars and Shapes, Carbon Rolled from “T’’ Rails A499
Steel Bars, Carbon, Merchant Quality, M-Grades A575
Steel Bars, Carbon, Hot-Wrought, Special Quality A576
Steel Bars, Carbon, Merchant Quality, Mechanical Properties A663
Steel Bars, Carbon, Hot-Wrought, Special Quality, Mechanical Properties A675
Steel Bars for Springs, Carbon and Alloy A689
Steel Bars, Carbon, Hot-Wrought, Special Quality, for Fluid Power Applications A695

Cold-Finished Carbon Steel Bars:
Steel Bars, Carbon, Cold-Finished, Standard Quality A108
Stress-Relieved Steel Bars Subject to Mechanical Property Requirements, Cold-Drawn Carbon A311/A311M

Hot-Rolled Alloy Steel Bars:
Steel Bars, Alloy, Standard Grades A322
Steel Bars, Alloy, Subject to End-Quench Hardenability Requirements A304
Steel Bars, Alloy, Hot-Wrought or Cold-Finished, Quenched and Tempered A434
Steel Bars, Alloy, Hot-Wrought, for Elevated Temperature or Pressure-Containing Parts, or Both A739

Cold-Finished Alloy Steel Bars:
Steel Bars, Alloy, Cold-Finished A331
Steel Bars, Alloy, Hot-Rolled or Cold-Finished, Quenched and Tempered A434
Steel Bars, Carbon, Hot-Wrought or Cold-Finished, Special Quality, for Pressure Piping Components A696
 
A purple for you CoreyPad. Hopefully this was a copy and paste operation for that much data.

Design for RELIABILITY, manufacturability, and maintainability
 
You really want to get to the product you are trying to analyze. I would look in the Worldwide Guide to Equivalent Irons and Steels by ASM first - it will list both product forms and equivalent alloys. Another good source is the listing of UNS alloys from ASTM/SAE - your alloys are UNS G10180 (1018), G10200 (1020), G41300 (4130), and G41400 (4140). This is usually a subset of what you will find in the Worldwide Guide, but it is useful especially if you do not have the first reference.
 