Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

What issues exist with welding on carbon steel lines that have been in anhydrous HCL service for 25 1

Status
Not open for further replies.

dutch1956

Chemical
Joined
Sep 7, 2012
Messages
5
Location
US
What safety & failure issues do I have to be concerned about on welding on the subject matter above.
If welding is not the route can lock ring flanges be used in this service.
 
Are you referring to a hot tap process or off-line, fully vented pipe system?
 
This line is off-line fully vented.
 
I don't see any weldability or safety issues. Make sure the weld preps have been cleaned and subject to NDT examination (surface) before welding.
 
I have noticed in the past that there are possibilities of subsurface discontinuties opening up under welding process. So I think that a UT thickness check of about 6" around the welded area be checked prior to welding.
 