Feb 24, 2016 #1 SEP2013 Industrial Joined Feb 24, 2016 Messages 2 Location US what in this description below = seamless? 8" SCH 10 SR 90 ELL A403 WP304L
Feb 24, 2016 #2 Don56 Mechanical Joined Feb 18, 2015 Messages 203 Location US Nothing. See A-403 There should be a "S" after the 304L. Upvote 0 Downvote
Feb 25, 2016 #3 LittleInch Petroleum Joined Mar 27, 2013 Messages 23,017 Location GB It's an elbow - default is that it's seamless?? As it's a forging. Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
It's an elbow - default is that it's seamless?? As it's a forging. Remember - More details = better answers Also: If you get a response it's polite to respond to it.
Feb 25, 2016 Thread starter #4 SEP2013 Industrial Joined Feb 24, 2016 Messages 2 Location US correct, according to A403 the description should read as 8" SCH 10 SR 90 ELL A403 WP304L-S Upvote 0 Downvote