We are installing some inclinometers deeper than 100m. We already had two expensive failures and the reasons for me are not clear and hard to accept. I was not at the site at that moment.
The 297ft inclinometer casing was installed inside a 7" steel casing. After grouted to the top, the driller started pulling out the 7" casing and it got stuck. The driller rotated the steel casing but the inclinometer casing got broken at 96ft at the junction. It was about 4 hours from the start of grouting to the failure of the inclinometer casing. the grout mxing was 35 gallon water + 25lb betonite + 94lb cement, a typical mixing for stiff soils.
One reason was given that turning the steel casing induced torsional force to the inclinometer casing through the grout.
Fluid does not transfer shear or torsional force. After about 4 hrs, can the grout transfer the torsional force to the inclinometer casing from steel casing due to cememntation of the grout? Or in fact the failure was casued by other reasons?
A test on the grout in the lab will be condcuted to check the strength growth over time. Meanwhile, would anyone give more suggestions, ideas and explanation?
The 297ft inclinometer casing was installed inside a 7" steel casing. After grouted to the top, the driller started pulling out the 7" casing and it got stuck. The driller rotated the steel casing but the inclinometer casing got broken at 96ft at the junction. It was about 4 hours from the start of grouting to the failure of the inclinometer casing. the grout mxing was 35 gallon water + 25lb betonite + 94lb cement, a typical mixing for stiff soils.
One reason was given that turning the steel casing induced torsional force to the inclinometer casing through the grout.
Fluid does not transfer shear or torsional force. After about 4 hrs, can the grout transfer the torsional force to the inclinometer casing from steel casing due to cememntation of the grout? Or in fact the failure was casued by other reasons?
A test on the grout in the lab will be condcuted to check the strength growth over time. Meanwhile, would anyone give more suggestions, ideas and explanation?