bholland,
I'm looking at a narrow groove, automatic orbital, GTAW deposited weld cross section and I can assure you that the HAZ is not smaller than similar weld deposits made with GMAW spray arc that I have examined. HAZ size is also be affected by the total heat input - travel speed being a primary variable and travel speed with GTAW, especially manual GTAW, is quite slow compared to other processes.