Hi,
I just developed welding procedures for ASME B31 piping using ASME Section IX welding code, I'm preparing to develop the same for wellhead piping, valves which I know is API 6A. Is there a different welding code for those or will it also be covered by ASME IX as long as the filler metal and material spec requirements are met?
Thank you.
I just developed welding procedures for ASME B31 piping using ASME Section IX welding code, I'm preparing to develop the same for wellhead piping, valves which I know is API 6A. Is there a different welding code for those or will it also be covered by ASME IX as long as the filler metal and material spec requirements are met?
Thank you.