Hello friends, please confirm what i understand as per QW- 424
If my PQR IS P4 TO P8 on BASE of this PQR CAN I Qualified to make WPS P4 TO P1, P4 TO P8 , P4 TO P3.
AS PER QW-424 BASE METALS USED FOR PROCEDURE
Base Metal(s) Used for Procedure Qualification ---- Base Metals Qualified
One metal from a P-Number to any metal from any other P- Number ----- Any metal assigned the first P-Number to any metal assigned the second P-Number.
please confirm
regards
stanly
If my PQR IS P4 TO P8 on BASE of this PQR CAN I Qualified to make WPS P4 TO P1, P4 TO P8 , P4 TO P3.
AS PER QW-424 BASE METALS USED FOR PROCEDURE
Base Metal(s) Used for Procedure Qualification ---- Base Metals Qualified
One metal from a P-Number to any metal from any other P- Number ----- Any metal assigned the first P-Number to any metal assigned the second P-Number.
please confirm
regards
stanly