engineermat
Mechanical
I have a super high pressure steam piping, which is 2.25Cr piping. It is going to be connected to a 316 SS Piping. We want to use welding or flange connection for these two different piping. The flow in the piping high pressure steam (959 DegF). We don't need to consider the galvanic corrosion for this condition since there is no electrolyte, right? These two piping can be welded or flanged, right?
Thanks.
Thanks.