Jun 22, 2011 #1 strauss2010 Mechanical Joined Jun 22, 2011 Messages 7 hi guys,i'm new with this forum just want to ask.,if there is any restriction in ASME regarding on welding or joining of SA36 with SA 516material.
hi guys,i'm new with this forum just want to ask.,if there is any restriction in ASME regarding on welding or joining of SA36 with SA 516material.
Jun 22, 2011 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US No. Upvote 0 Downvote
Jun 22, 2011 #3 Fizza453 Mechanical Joined Jun 22, 2011 Messages 262 Location AE SA-36 plate for pressure retaining parts may only be used within the limitations of UCS-6(b) in Section VIII-1 construction. Upvote 0 Downvote
SA-36 plate for pressure retaining parts may only be used within the limitations of UCS-6(b) in Section VIII-1 construction.
Jun 22, 2011 Thread starter #4 strauss2010 Mechanical Joined Jun 22, 2011 Messages 7 Thanks guys for the rply,i used A36 plate as a insulation support. Upvote 0 Downvote
Jun 22, 2011 Thread starter #5 strauss2010 Mechanical Joined Jun 22, 2011 Messages 7 And also as what Fizza453 it conform with the limatation under UCS 6,it does not content lethal substance and the thickness of plate is only 10mm it does not exceeds the requirements under UCS 6 Upvote 0 Downvote
And also as what Fizza453 it conform with the limatation under UCS 6,it does not content lethal substance and the thickness of plate is only 10mm it does not exceeds the requirements under UCS 6
Jun 26, 2011 #6 GenB Mechanical Joined Oct 24, 2003 Messages 1,362 Location US supports? that's even better as it does not contain pressure... Upvote 0 Downvote