My question is does AWS D1.1 allow welding of PQR coupons to be outsourced, for example to a test facility, or does the welder have to be an employee of the contractor qualifying the procedures?
 
The latter is permitted. The former is not permitted.


Best regards - Al
 
Preparation and testing of mechanical specimens may be outsourced. Welding of the PQR coupon and associated certification of the PQR must be performed by the individual contractor or manufacturer.
 
Thanks a lot, that's what I thought but needed some back up.
 