Who can review and approve Welding procedure specification for a Pressure vessel fabrication Project?
What all qualification is required?
PQR approved and stamped by Lloyds Register inspector,is this recognised internationally?
Thanks,
DV
 
Replies continue below

Recommended for you

Your question is too vague - more information required.
Is it an ASME vessel ? - If so what is the location for installation ?
Is the vessel subject to PED ?
More information - more help.
And AWS is Structural - not the best place to post a PV question.
 
You could have Jesus himself sign it and it won't be acceptable. The company has to certify. In all seriousness, A Lloyds signature is always a good thing, but you need to sign (certify) as well.
QW-200.2
QW-201
 