I want to weld a 1.5"weldolet to 8" pipe. The welder is qualified in 8" pipe full GTAW. This welder can weld this weldolet? Code is asme sec IX. This is a groove weld not fillet.
Also thickness also need to consider?

Menon
 
Replies continue below

Recommended for you

8" Pipe performance will qualify 2-7/8" Min. Outside Diameter. - Table QW-452.3
Bonney Forge 1.5" Weldolet OD = 2-7/8" - Internet
Bonney Forge 1.5" Weldolet Standard Weight Wall Thickness: 7/16"
8" Pipe Sch Std performance - .644" WM Qualified.


 