Dec 22, 2014 #1 fabengr Structural Joined Nov 29, 2009 Messages 30 Location CA I have an application where I need to weld some mild steel plates to ASCE 70# rail. What AWS standard do I need to be looking at?
I have an application where I need to weld some mild steel plates to ASCE 70# rail. What AWS standard do I need to be looking at?
Dec 30, 2014 #2 weldstan Materials Joined Jun 24, 2011 Messages 2,806 Location US I believe that AWS D15.2 addresses the issue. Upvote 0 Downvote