Jul 20, 2017 #1 stan000 Mechanical Joined Jul 31, 2014 Messages 121 Location CA in "welding continuity log" is that necessary to have S.A.W Process to show continuity of welder for SAW. regards stanly
in "welding continuity log" is that necessary to have S.A.W Process to show continuity of welder for SAW. regards stanly
Jul 20, 2017 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Yes. You have to show the welder has welded within the last 6 months using the process they qualified. Upvote 0 Downvote
Yes. You have to show the welder has welded within the last 6 months using the process they qualified.