Hi Expert,
I Have some question regarding Clad Pipe 625, Is it possible to use 625 Filler wire (ERNiCrMo-3) on the Root and Hot Pass only , then Carbon steel Wire (i.e. ER70S-6) for the subsequent welding (Fill and Cap) ?,I there any problem with dilution? (Metallurgical perspective)
we're useing GTAW with Ar 99.997% as shielding and backing gas.
I just think , are we need bridging filler metal (ER309L) as bridging filler between 625 weld metal and Carbon Steel Weld Metal ?
Thanks
I Have some question regarding Clad Pipe 625, Is it possible to use 625 Filler wire (ERNiCrMo-3) on the Root and Hot Pass only , then Carbon steel Wire (i.e. ER70S-6) for the subsequent welding (Fill and Cap) ?,I there any problem with dilution? (Metallurgical perspective)
we're useing GTAW with Ar 99.997% as shielding and backing gas.
I just think , are we need bridging filler metal (ER309L) as bridging filler between 625 weld metal and Carbon Steel Weld Metal ?