Dear All,

Does anyone know a reliable supplier for welded or seamless alloy pipes? We trying to source sizes from 1/2" to 16".
Project will be in US so local supplier is preferred.

Thanks in advance
 
Maybe cancel the question here, and move it to the Pipelines, Piping & Fluid Mechanics forum?

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Thanks Steve,
Tried already in others
 
The question of the day is how much volume?
And just standard pipe or anything special about it?
I know of a US source that will weld up to 4.5" OD (4NPT).
Getting seamless in anything over 1NPT in the US could be tough.
You could go Japan or Northern Europe for seamless, if you have a lot of time.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Hi EdStainless,

Specs are ASME 16" Sch10 since the media is exhaust gas. Qyt not too much like 35m
8" around 10m
6" around 20m
2" around 40m
Smaller size will be seamless anyway.
European market has log delivery time ~ 6 months
We bought from China in short time but material was in stock as plates. So we were lucky. Also high risk of getting fake material from China unless you have 3rd party involved from day 1 until packing.

 