Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

WELDING OF CR-MO STEEL P9 GRADE WITHOUT PWHT - USING 625 INCONEL FILLER METAL 1

Status
Not open for further replies.

GabrieleB

Petroleum
Joined
Feb 4, 2009
Messages
84
Location
IT

A supplier of Heat exchanger made in SA 387 Grade 9 steel to avoid the PWHT is going to use a filler metal ERNiCr-3 (alloy 625).
The welding process is made with 4 passes of GTAW (thickness qualified 9mm).

It is sufficient this process to avoid the PWHT that is usually mandatory required for Grade 9 materials (9%Cr-1Mo) P-NO 5B?

Waiting for a kind response.
 
Ask the supplier to quote where it is permitted in ASME VIII Code or Code Case thereto. This technique was originally developed by EPRI for repairs to P91 boiler tubes.
 