Several Carpenter 20(Alloy 20)tubes are to be welded to a 316L stainless steel raised face pipe flange.

This is basically a P45 to a P8 weld.

Weld material for the 316L material is SFA-5.9 ER316L.

Weld material for Carpenter 20 is SFA 5.9 ER320LR.

What weld material should be used when welding Carpenter 20 to 316L stainless steel?
 
Replies continue below

Recommended for you

We used SFA 5.9 ER320LR for welding 316 to Carpenter 20 Cb-3 for use in a very corrosive process.
 
We've used ER320LR, ER309LMo, and ERNiCrMo-3 for these joints depending on Owner requirements.

 