Welding after Hydrotest for Tank

Status
Not open for further replies.

hmzM

Petroleum
Joined
May 16, 2003
Messages
14
Location
SD
Dear All, I have one problem. A tank has been hydrotested but unfortunately the contractor miss to install (welding)anode bed inside the tank (in the drawing, not mentioned about anode bed but mentioned in the contract requirement). Did the contractor still need to carry out the hydrotest or not? Which clause needs to refer?
 
Comeback with some physical information as to code of construction and material of construction.
How much welding and what connection type?
 
API-650 has recently been revised to permit post-hydro minor welding on tank shells. There are lots of limitations and special rules to follow. Check it out, it may be useful to you.

Steve Braune
Tank Industry Consultants
 