Jan 3, 2006 #1 donnaj Mechanical Joined Sep 6, 2005 Messages 12 Location US Can someone tell me what is the correct filler metal for welding 446SS? Thanks
Jan 3, 2006 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US It depends on your application - service temperature. The Ni-base filler metals are your best bet and austenitic stainless filler metals will work. See the information below; http://www.suppliersonline.com/propertypages/446.asp Upvote 0 Downvote
It depends on your application - service temperature. The Ni-base filler metals are your best bet and austenitic stainless filler metals will work. See the information below; http://www.suppliersonline.com/propertypages/446.asp
Jan 4, 2006 #3 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US You might want to give these people a call. I have seen their electrodes used on 446 SS. Don't remember the type but it worked. http://www.eurekaweldingalloys.com/default.asp Upvote 0 Downvote
You might want to give these people a call. I have seen their electrodes used on 446 SS. Don't remember the type but it worked. http://www.eurekaweldingalloys.com/default.asp