Dear Experts,

Our plate welders are qualified with SMAW process. We plan to used FCAW (pre-qualified WPS), is there a required re-qualification for our welders?
 
Replies continue below

Recommended for you

Yes, FCAW is a different welding process.

Best regards - Al
 