What is the magnitude of the effect on weld strength of welding a nitrided part? The formation of iron nitrides will have some effect but I have not been able to find values suitable for design calculations.
A little background into my application:
A nitrided 1010 pin is welded all around to an A36 plate with 29S wire. The loading condition results in a max stress of ~18000 psi on the weld.
Since the stress on the weld is low it would probably be strong enough even with the nitrided part but I don't want to make a design decision on a gut feeling.
If anyone could point me in the direction of reference material I would really appreciate it.
A little background into my application:
A nitrided 1010 pin is welded all around to an A36 plate with 29S wire. The loading condition results in a max stress of ~18000 psi on the weld.
Since the stress on the weld is low it would probably be strong enough even with the nitrided part but I don't want to make a design decision on a gut feeling.
If anyone could point me in the direction of reference material I would really appreciate it.