Dear weld experts,

May apply strength weld to the joint between SA-266Gr2 of tube sheet and SA-312TP316L of tubes?

Thanks
 
It cannot exceed the weaker of the two materials.
In this case that would be annealed 316L.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 