Dear All,
We have qualified a two welder in a single specimen(GTAW+SMAW).Qualification thickness will be based on the deposited weld metal thickness or as per the specimen thickness ?
Ie out of 18 mm thk , GTAW - 4mm and SMAW 14 mm . So the GTAW welder qualified for unlimited thickness or 3/4" as per 9.1.3.
Size 6" 18 mm thk
Regards,
Ratheesh N
We have qualified a two welder in a single specimen(GTAW+SMAW).Qualification thickness will be based on the deposited weld metal thickness or as per the specimen thickness ?
Ie out of 18 mm thk , GTAW - 4mm and SMAW 14 mm . So the GTAW welder qualified for unlimited thickness or 3/4" as per 9.1.3.
Size 6" 18 mm thk
Regards,
Ratheesh N