I need a good resource to find the weight of Chromoly materials. For example F22 or F91. Thank you.
 
Thank you metengr. Is there a resource you could suggest? I'm sure there is a reason, but all of the calculators that I can find do not recognize Chromoly. I am guessing that this is probably because it is not a stand alone alloy.
 
I believe you can just use the standard weight for carbon steel for these alloys. There won't be substantial weight difference.
 
Thank you to all. I will check out matweb.com also.
Have a great day.
Jonathan
 
If you cannot find density for a specific alloy, look for properties of a more popular alloy with similar composition. In this case, 410 stainless. The ferritic and martensitic stainless steels (and even the austenitics) do not vary much from the 0.28 lb/in3 of carbon steel.
 