where can I find a good source for building materials weights.e
for example unit weight of sheeting galvanize ,plywood etc by a recognize authority
 
Replies continue below

Recommended for you

AISC steel construction manual has this info. Don't forget: There's always google.
 
Usually MSDS sheets will have density or specific gravity included on them.
If it's critical, look up two or three different brands.
 
The commentary to Chapter C in ASCE 7-10 (and earlier versions) has a fairly comprehensive listing of building material weights.
 