fujit
Mechanical
- Apr 16, 2009
- 7
We have the following valve and service -
Pressure Class 900
Max Valve Pressure – 2250 psi
Max Valve Temperature – 100F
Max Valve Pressure at Max Temperature – 2250 psi
Valve Service – Propylene
I am looking for the following information -
- Compatibility of Devlon V seat material with the propylene service
- Compatibility of PEEK seat material with the propylene service
Please reply with reference for information.
Thank you.
Pressure Class 900
Max Valve Pressure – 2250 psi
Max Valve Temperature – 100F
Max Valve Pressure at Max Temperature – 2250 psi
Valve Service – Propylene
I am looking for the following information -
- Compatibility of Devlon V seat material with the propylene service
- Compatibility of PEEK seat material with the propylene service
Please reply with reference for information.
Thank you.