Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Does N06040 Casting for Valve Body Require NACE MR 0103 Qualification in Sour Caustic Environment? 1

Status
Not open for further replies.

Hajiwaji

Mechanical
Joined
Jan 1, 2023
Messages
24
Location
SA
For caustic environment containing H2S and meet the definition of sour as per NACE MR 0103, does require testing and qualification for ssc? N06040 is not listed in NACE MR 0103 section 14.
 
Check 14.1.1.2 against the base requirements for A494 N06040. Then review clause 11.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Thank you Dr. Jones.

N06040 does not meet the chemical composition requirements in clause 14.1.1.2 of NACE MR 0103, hence qualifications are required as per clause 11.
 